ISO 2069:1976
w
ISO 2069:1976
6852

Résumé

This method is applicable to products having Ca contents greater than 0,003 % (m/m). The principle consists in dissolution of a test portion by the influence of hydrochloric acid under pressure. Addition of sodium ions to promote and to stabilize the emission of calcium, and of lanthanum ions or triethanolamine to increase the sensitivity. Aspiration of the solution into an acetylene-dinitrogen monoxide flame and photometric measurement of the absorption of the 422,7 nm line emitted by a hollow-cathode calcium lamp. For the determination of higher CaO contents (over about 0,03 % (m/m)) an acetylene-air flame can be used. Replaces ISO Recommendation R 2069-1971.


Informations générales 

  •  :  Annulée
     : 1976-08
  •  : 1
     : 4
  •  : ISO/TC 226 Matériaux pour la production de l'aluminium de première fusion
  •  :
    71.100.10 Matériaux pour la fabrication de l'aluminium

Vous avez une question?

Consulter notre FAQ

Service à la clientèle
+41 22 749 08 88

Horaires d’ouverture:
De lundi à vendredi - 09:00-12:00, 14:00-17:00 (UTC+1)

Suivez l'actualité de l'ISO

Inscrivez-vous à notre Newsletter (en anglais) pour suivre nos actualités, points de vue et informations sur nos produits.